Recommended products:Water Based Bentonite For Coating— SMP
HZinfo2025-05-21 09:46
SMP additive is a purified, nanometer modified and viscosity improved montmorillonite clay. It is off-white, soft, nonpoisonous and tasteless. Because of excellent expansibility, gel dispersing ability, suspension, thickening and thixotropic performance, it can be used as anti-settling agent, latex stabilizer and Rheology Modifier in water based system. Besides, it also has the property of good absorption, iron exchange and cohesive in water based system.
SMP high purity nanoclay’s main chemicals are SiO2 and Al2O3. Two layers of silicon-oxygen tetrahedron and one layer of aluminium octahedron lamellar stack to form montmorillonite clay particles. The thickness of single layer is 0.96mm. Electronegativity exists between layers and they can exchange ions and get modification. .Those layers have good thermal stability and help to reach excellent flame retardant and barrier propertity.
Applications
Should be used |
For use |
Daily use chemicals , such as toothpastes, facial mask, detergents. |
Thixotropic thickening, adsorption decontamination |
Latex paints, Water borne inks, ceramics glaze |
Thickening and stabilization, latex stability, rheological additives |
Medicine Industry |
Suspension, bonding and adsorption |
Spin |
Textile industry and dye printing |
Paper industry |
Scattered, Xu Ning, homogeneous |
Polymeric material |
Synergistic flame retardant, improve the mechanical performance, improve the barrier properties |
Quality Index
TYPE/INDEX |
SMP |
COLOR/FORM |
Off-white and light yellow,finely powder |
MOISTURE,% |
≤10.0 |
pH value (2% dispersion) |
9.5±0.5 |
Density,g/cm2 |
2.2 |
FINENESS(-200mesh),% |
≥95 |
Viscosity(5%, 60rpm),mpa.s |
≥100 |
Instructions
Pre-gel usage: SMP is slowly added to water with 25-35℃ temperature with constant mixing, increase the mix speed to 1500-2000rpm for 20-30min to avoid clumping and reach full dispersing. Then place it for 8-12h for use. Put this gel into the whole system with constant mixing until complete dispersing (pre-dispersing concentration of montmorillonite clay in water is 8-15%). Using pregel has better performance than add powder directly.
Packing and storage
Outer package is leather bag, with inner package of two layers of polyethylene film, or paper bag. Standard quantity is 25±0.25kg or customization. Stored in dry and ventilated places under the temperature of 0-30℃. Shelf life: 24monthes.
MORE HZinfo
- Brief Report on the Economic Operation of China's Coatings Industry in 2025
- In 2025, despite the Chinese coatings industry making solid strides on the path of high-quality development, the output of coatings saw a slight decline due to the dual pressures of weak downstream de
-
2026-06-04
- Market Report of the Raw Materials for Coatings and Waterproofing in 2025
- In 2025, China's coatings procurement costs will exhibit a moderate downward trend with structural differentiation, while the paint and raw material market will display a distinct "cost-price" diverge
-
2026-06-04
- Jinbaoli Deeply Cultivates the SpecialCoating & Resin Track
- Whether it is employees, suppliers or customers, only when the three parties are united and sincerely solve problems for each other can a positive cycle be formed to survive the industry cycle.
-
2026-06-04


English
简体中文
Русский
إنجليزي