Paint Defects—— Dry Spray
2025-02-10 14:18
Dry Spray
1.Description
Rough and uneven finish to the surface of the paint film where the particles are insufficiently fluid to flow together. This defect is normally limited to small areas.
Figure 1 Schematic diagram of dry spraying
2.Probable Causes:
Incorrect spray application i.e. gun distance. Also associated with fast drying products and too high an application temperature.
3.Prevention:
Use correct coating application equipment and techniques. Use a slower drying solvent or solvent blend. Follow recommended application procedures.
4.Repair:
Allow the paint to dry and then sand. After sanding, and depending on the magnitude of the defect, respraying or polishing will be necessary.Abrade and remove any loose dryspray and re-apply coating or topcoat.
MORE HZinfo
- Architectural Coating: Ceramic Sand Coating, Showcasing The Dignified And Elegant Beauty Of Buildings
- As a facade decoration material that highlights the dignified and elegant beauty of buildings, Ceramic Sand Coating boasts numerous highlights.
-
2025-09-12
- Green, Innovation, Cooperation | The Journey of Cadello at the International Coatings Expo Concludes Successfully
- This exhibition not only showcased Cadello's technical and product excellence, but also provided innovative insights for the industry's green transformation.
-
2025-09-12
- Recommended products:Dingrui New Materials Copper Chromium Black - Excellent Chemical Resistance, Outdoor Durability, Lightfastness, and Thermal Stability
- Copper chromium black is a blue-phase black pigment calcined at high temperatures.
-
2025-09-12