Paint Defects—— Dry Spray
2025-02-10 14:18
Dry Spray
1.Description
Rough and uneven finish to the surface of the paint film where the particles are insufficiently fluid to flow together. This defect is normally limited to small areas.
Figure 1 Schematic diagram of dry spraying
2.Probable Causes:
Incorrect spray application i.e. gun distance. Also associated with fast drying products and too high an application temperature.
3.Prevention:
Use correct coating application equipment and techniques. Use a slower drying solvent or solvent blend. Follow recommended application procedures.
4.Repair:
Allow the paint to dry and then sand. After sanding, and depending on the magnitude of the defect, respraying or polishing will be necessary.Abrade and remove any loose dryspray and re-apply coating or topcoat.
MORE HZinfo
- BDS Makes a Strong Impact at 2026 Guangzhou Custom Home Fair with “Total Home Coating, One-Stop Solution”
- The four-day 2026 Guangzhou Custom Home Fair & Light High-End Customization Exhibition concluded successfully on April 1.
-
2026-04-01
- Shunde Coatings' Answer for the 15th Five-Year Plan
- Zhang outlined a vision for high-quality development in the Shunde coatings industry.
-
2026-04-01
- Toray Industries, Inc. Announces Surcharge Pricing For Selected Products
- Emergency Introduction of Surcharge Pricing in Response to Surge in Raw Material Costs Amid Middle East Tensions and Strait of Hormuz Blockade
-
2026-04-01


English
简体中文
Русский
إنجليزي